production- galvanic coating
"Proper protection is the key to excellence."
Alkaline zinc – Fe/Zn8/An/T2
- Electrolytic protective coating ZN alkaline,
- Transparent chromate passivation free from Chromium (VI),
- Corrosion resistance is a minimum of 72 hours to red corrosion in a salt chamber,
- In order to better protect against corrosion and increase resistance at higher temperatures, we protect all coatings with a sealant (varnish).
Zink-Nickel – (Fe/ZnNi8/Cn/T2)
Alkaline alloy coating with additional sealant.
- Very high corrosion resistance (up to 1200 hours to red corrosion in a salt chamber),
- Details covered with this coating do not create corrosion cells when combined with aluminum,
- High corrosion resistance to temperature changes or operation at elevated temperatures,
- Lower emission of zinc compounds into the environment during use of products with this coating,
- Increased hardness compared to pure zinc coatings and other zinc alloy coatings, ensuring significantly increased resistance to mechanical damage.